Why aromatic resin has poor UV resistance?

Why aromatic resin has poor UV resistance than aliphatic and cycloaliphatic? For aromatic cyclic diacid ,why ortho , meta substitution more durable than para?

Most recent answer

All Answers (4)

21st Jan, 2018
Gyorgy Banhegyi
Medicontur Medical Engineering Ltd.
Aromatic resins absorb UV more strongly than cyclolaliphatic ones, their functionalizatio or decomposition is easier.
1 Recommendation

Similar questions and discussions

Related Publications

Article
Full-text available
The knowledge of the factors affecting the susceptibility of asphalt to aging can be of help when selecting the asphalt binders for the construction of durable pavements. Investigated were, the aginginduced changes in the chemical composition and colloidal nature of asphalts differing in origin and technology. It was shown that the course of the ch...
Article
OSB panels were manufactured with a mixture of pine and cypress heartwood and lignin and tannin based resins in order to propose an eco-friendly wood composite. The resistance of OSB panels against Reticulitermes santonensis was tested according to EN 118 and EN 117 as well as in a field test. OSB made from cypress showed more resistance against th...
Technical Report
Full-text available
Freeze-thaw resistance is a key durability factor for concrete pavements. Recommendations for the air void system parameters are normally: 6 ± 1 percent total air, and spacing factor less than 0.20 millimeters. However, it was observed that some concretes that did not possess these commonly accepted thresholds presented good freeze-thaw resistance...
Got a technical question?
Get high-quality answers from experts.