Started 27 March 2024

PZT (piezoelectric ceramic) precision injection valve ?

Hi,
I have no expertise in precision fluid mechanics and PZT (piezoelectric ceramics). Based on the foundation of precision manufacturing, I have recently been designing a PZT (piezoelectric ceramic) precision injection valve for high speed and precision injection of solder paste (5 #, viscosity solder paste).
Therefore, it is necessary to know the linear relationship between the 48V voltage of the "inverse piezoelectric effect" generated by the PZT (piezoelectric ceramics) and the tungsten steel firing pin (AF 312 material, diameter 1.5mm) and the nozzle (AF 312 material, internal hole less than 0.1mm), the core components of the precision injection valve.
As a rule of thumb, the deformation elongation of PZT (piezoelectric ceramics) is 32±0.2μm and the voltage is 48V (To my knowledge).
(1)How to further improve the inverse piezoelectric effect of PZT (piezoelectric ceramics) in order to achieve the application of piezoelectric ceramic injection valves and other precision injection devices ?
(2)How to further Improve response frequency and efficiency ?
Please suggest me something. Thanks.
Thank you for sharing and helping,
Best Regards,
Jiabin Xu (Jia-bin Xu)
Harbin Institute of Technology (HIT)
School of Mechatronics Engineering
Timestamp/ Time Line: 2024-03-27, Wednesday, Evenfall

All replies (1)

Vladimir Kubov
Petro Mohyla Black Sea National University
Do you have any working prototype of the device? What function should an ultrasonic generator perform? What is the configuration of the working chamber and the position of the nozzle in this chamber?
If there is no prototype, then this is a huge research work, with problems unknown in advance. The theory can appear only later, when experimental data appear.
1 Recommendation

Similar questions and discussions

How are the coordinates of the straight lines defined in the Abbe diagram?
Question
Be the first to answer
  • Ya-Fan ChenYa-Fan Chen
I would like to plot the Abbe diagram using Plotly.
But some of the lines are not integers but floating numbers.
I wonder how these blue lines defined in the Abbe diagram?
is there any reference source to these coordinates?
CFP: 2024 5th International Conference on Material Chemistry and Composite Materials (MCCM 2024) - Decemeber,2024
Discussion
Be the first to reply
  • Chuliang WuChuliang Wu
2024 5th International Conference on Material Chemistry and Composite Materials (MCCM 2024) will be held on Decemeber 27-29, 2024 in Xiamen, China.
---Call for papers---
The topics of interest for submission include, but are not limited to:
1. Material Chemistry
Electrochemical Materials
Surface Chemistry
New Energy Materials
Surface Chemistry
Chemical Physics
Optical materials
......
2. Composite Materials
Magnetic Materials
Computational Materials Science
Nanotechnology and Materials
Ceramic and Glass Materials
Materials Physics
Materials for Energy Catalysis
......
---Publication---
All accepted conference papers will be published in the Journal of Physics: Conference Series (JPCS) (ISSN:1742-6596) which will be submitted to EI Compendex and Scopus for indexing.
---Important Dates---
Full Paper Submission Date: November 30, 2024
Registration Deadline: December 16, 2024
Final Paper Submission Date: December 23, 2024
Conference Dates: December 27-29, 2024
--- Paper Submission---
Please send the full paper(word+pdf) to Submission System:

Related Publications

Article
Full-text available
Lead-free piezoelectric ceramics based on bismuth sodium titanate (BNT) -barium hafnate titanate (BHT) were prepared by a two-step synthesis process. The final BNT-BHT ceramics sintered at 1180oC for 2 h in air showed a perovskite structure with high density. The morphotropic phase boundaries (MPB) were found in BNT based piezoelectric ceramics wit...
Article
PZT/NiTi composites were prepared by the method of depositing NiTi films on the PZT substrates by magnetron sputtering method. The phase structure and hetero-structure of the composites were examined by using X-ray diffraction (XRD) and scanning electron microscope (SEM). A phase method was utilized to research on the damping capacities of PZT/NiTi...
Got a technical question?
Get high-quality answers from experts.