Synthesis procedure.

All Answers (2)

16th May, 2014
Dmytro Bobukhov
Ukrainian State University of Chemical Technology
The common oxidation state for rhodium is +3, so previous equations are not correct. As I know Rh will not react with nitric acid, so the only way to get pure Rh2O3 is oxidizing under the high temperature (600-700 C). But rhodium should be powdered. But if you need to get rhodium(III) salt, it will be better to obtain RhCl3 by chlorination under high temperature (500 C):
2Rh + 3Cl2 → 2RhCl3
You can also convert rhodium to Rh2(SO4)3 reacting powdered rhodium with molten KHSO4, but this reaction is very slow.
Anyway from RhCl3 or Rh2(SO4)3 you can get rhodium(III) oxide hydrate (Rh2O3 x 5H2O) or rhodium(III0 hydroxide by the reaction with NaOH and then get rhodium(III) nitrate.

Similar questions and discussions

Related Publications

Article
Thèse (Ph. D.)--Université de Montréal, 1989. "Thèse présentée à la Faculté des études supérieures en vue de l'obtention du grade de Philosophiae Doctor (Ph. D.) en chimie." Microfilm du manuscrit.
Article
Inamide zeichnen sich durch ein außergewöhnlich ausgefeiltes Gleichgewicht von Stabilität und Reaktivität aus. Sie bieten eine Vielzahl von Möglichkeiten zur Einführung einer Stickstoff-Funktionalität in organische Moleküle und werden zunehmend als besonders nützliche und vielseitige Bausteine für die organische Synthese angesehen. Aktuelle Durchbr...
Got a technical question?
Get high-quality answers from experts.