Figure 3 - available via license: Creative Commons Attribution 3.0 Unported
Content may be subject to copyright.
shows the maximum flame temperature on the field strength dependences. At E , an increase in the maximum flame temperature is observed: for rubber by 60 °C, for polystyrene by 270 °C, for polypropylene by 80 °C with field strength values up to 150 kV/m. For polyethylene, the temperature does not increase within the experimental error. At E
Source publication
Polymer waste disposal of is one of the most pressing problems of our time. The incineration method is widespread, but it has its drawbacks. Problems during the polymer waste combustion, which include low combustion efficiency, combustion products toxicity, significantly reduce the possibility of waste disposal incinerators using. In this regard, t...