Université Clermont Auvergne & Institut Universitaire de France (IUF)
Question
Asked 13th Mar, 2015
How much should we deacetylate chitosan for manufacturing bandage?
I want some information specially some papers about deacetylation of chitosan for manufacturing bandage
All Answers (3)
Hi,
For your topic, you could read this review on chitosan.
Regards,
Cédric
Article Chitosan as an adhesive
Similar questions and discussions
Related Publications
Apstrakt: Sklonost tekstilnih materijala da se gužvaju smanjuje se doradnim procesom kada se u amorfnoj fazi inkorporiraju umrežena jedinjenja koja poboljšavaju oporavak materijala nakon otklanjanja sile pritiska. Konvencionalna jedinjenja na bazi formaldehida za obradu zbog nepovoljnog delovanja na zdravlje čoveka sve više se supstituišu novim jed...
The wide array of tissue engineering applications exacerbates the need for biodegradable materials with broad potential. Chitosan, the partially deacetylated derivative of chitin, may be one such material. In this study, we examined the use of chitosan for formation of porous scaffolds of controlled microstructure in several tissue-relevant geometr...