Question

Could anybody tell me if there are natural sources of Polycarboxylate Ether.

It's used as a superplastisizer in SCC. I'm trying to create it in the lab

Topics

0 / 0  ·  4 Answers  ·  145 Views

All Answers (4)

  • Ignatius:

    I have offered the following to others here: the Internet is your friend; use it. Please see the following

    GEOPOLYMER HAVING NOVEL ORGANIC COMPONENTS AND ...
    www.faqs.org/patents/app/20110219985 - Cached
    2 days ago – Conventional geopolymers can be made from natural sources of ... [0022] The steps above can produce polycarboxylate ethers (PCE) or just ...

    When you open this page, go down to [0021] to [0023] , first. These more directly pertain to your concerns.

    Now, 'google' the following search term which is derived from your request:

    "natural sources of Polycarboxylate Ether"

    If you do that soon, you may be surprised by the very first search result listed.
    Certainly, you will find much more documentation which may assist you.

    Good hunting.
  • Rongbing Bian · Nanjing University
    All raw materials for pc is from oil and chemical company, no naturally source for pc. Pc is designed by chemist and engineer in plant.